I set my layer temps with the Process, and not the start gcode
you can set different temp's for say layer 1 layer 2 for both bed and hotend
just go to edit process settings - temp..
just an update, i got some real good prints now with petg, but ended up using kisslicer the finish was 60% or more better, and i ended up drawing my own supports in the model and turning supports off in the slicer they came off real easy and no part breakage...
Everything seems solid can't peel anything off don't see any separation all the way up, my thought is something to do with supports... where it seems to break is a support area, in the bottom extrusion slot and it is the only section that has supports. I tried it without any support but it's about a...
I attached the stl.. Its for a printer i am working on and it is sorta L shaped and the extrusions slide in both ends. I printed it standing up so it only needs supports in the bottom extrusion slot, i have redrawn it now to make the walls a little thicker, haven't tried printing the newer version, ...
i am using esun have tested from 240 to 250, it looks like the print is good i don't see any separation or space between layers i will post a pic of the broken part.. have to get the camera out..
I have been trying to print a part in PETG, the print looks good. nice finish and all.. But seems like it always has a weak spot one corner always breaks off, i though PETG was suppose to be a little flexible and tough. Printed 3 parts all the same results.. I printed the part in ABS and PLA and bot...
I attached a couple pic's of a part in ABS i can't seem to get it honed in right, i have PLA printing fine. The pic's are printed at 260 and 250%c but around the though holes seems to be hollow the width of the hole. I have printed a square cube 25mm and that looks good all around, just seems to get...