After polishing with sandpaper 無題3.jpg The white part is a state in which garbage is clogged in a small groove. Because the extrusion width was made large on the right side, the groove almost disappeared. As shown in the picture below, many grooves may occur. P1011418.JPG Filling these grooves with ...
I made a program to convert the GCODE file and printed it.
The conversion target is InnerPerimeter and SolidLayer.
Left: Normal extrusion width
Right: 120% extrusion width
I would like a solid layer extrusion width designation option. The solid layer has slightly small grooves. In order to make a flat surface for painting, it is necessary to fill the groove with putty. If the extrusion width of the solid layer is made wider, the groove is buried, which makes work very...
... Does Combin Option make a problem occur? ... Yes, if the number of combin layer is higher than a half extrusion width it becomes critically. You are printing a layer high of 0,1 mm with a moderate speed and low temperature. Then the GCode changes suddenly to print infill and it needs the triple...
Thank you for advice. > I your case I would do just let it do one 1 shell and increase the max print width for single extrusion. preview each layer >and see of the is fewer retractions I have already tested them. Max Print width is 200%. >Your A 0.4-0.10 FFF has only 230° for ABS-filament, that to c...
Very small infill printing produces a lot of retraction, so the gear of the extruder scrapes filaments. For this reason, extrusion failure of the filament occurs. It is likely to occur with small nozzles such as 0.2 mm.
Process name = A0.4 - 0.10mm (R)
Line Range Max = 29197