I have searched through the guides but have not been able to solve this issue. IT seems that on think parts the printer print s very nicely. again on thick parts all is good. However if I have a part that is around 2mm I get really weird sidewall 'patterns'. I have tried printing at lower temps and reducing the extrusion multiplier. I have checked the e steps and its bang on
Printing PETG at 240 degrees
You can see though that where the text is on the headband it seems to print much better