Page 1 of 1

Top layer quality problem

Posted: Wed Sep 23, 2020 3:06 am
by alshaerahmed
Hi ,

I have been using cura before i start using s3d , in cura there was an option of ironing which produce great top layer surfcae , in s3d i increased the top layer to 6 and still getting poor quality in top layer , please any advice would be appreciated.

thanks

Re: Top layer quality problem

Posted: Thu Sep 24, 2020 10:01 am
by S3D-Jake

Re: Top layer quality problem

Posted: Wed Dec 23, 2020 9:16 pm
by 3dAngelo
Hello, I'm having a problem with my top layers not being printed perfect. The blue lines on top seem far apart from each other (Seen in Picture 1), When printed you can see the teeth, top forehead and eye top layers are not being fill in all the way. But the rest of the print is amazing.

Please help, Thank you,

Mac
20% Fill
0.4 Nozzle
0.2 Layer
Mat. PLA
50mm Speed

Re: Top layer quality problem

Posted: Sat Jan 02, 2021 4:23 am
by 3dAngelo
Thank you for your help!!!!! I see that I have to lower my layer height. Sorry new to 3d printing!