Hey guys - new user but I have a dremel 3d20 printer and I finally am getting decent prints except I get a tiny line on the top layer. I messed with retraction by turning off ooze control behavior in advanced but in the extruder settings I have this attached.
The line is VERY faint but it's still there and this time is like dotted line blob like but not that much plastic. Any tips on this?
If you're getting drag marks across the top flat surface...which I don't think I can see on your photos....then you need to add Vertical Lift....which you have set as zero!
What I can see in your photos is the result of thick layers leaving a "staircase" effect on sloping surfaces. You're not going to eliminate this effect....but you can reduce it significantly by printing with as thin a layer as your printer will print at.
Your print also, to me, exhibits signs of slightly over-extrusion....and looking at your Extrusion Multiplier, set at 1.00 for PLA might be a little high.
The spaghetti along the side of the finger is probably due to un-supported printing....the solution being to add supports.
Can't offer much more as what I have offered so far is based on interpretation of two photos....and little else!
Jumping from 1.0 to 0.9 is far too big a jump for changing the extrusion multiplier. Change in steps of 0.01. I'd aim to get to around 0.95......but that's a complete generalisation!!! Its make a small change ,,,,,and look to see if there is any difference. Make another small change.....and see what happens then.
Try a vertical lift of 1mm....and again, adjust in small steps. NEVER jump from one extreme to another!
And according to Google searching, your printer's minimum layer thickness is 0.1mm. I'd use that for fine finishes...
And a final thought. NEVER make a change without understanding the effect of making the change beforehand. Maddly tweaking settings about is not the way to understand what settings do. And don't change two settings at the same time....if there's a difference, which change made the difference???